Show All Results

Hot-Dip Galvanizing for Corrosion Protection: A Specifier's Guide

Corrosion and repair of corrosion damage are multi-billion dollar problems - the latest estimates show metallic corrosion costs the United States approximately $423 billion annually ($52 billion in Canada), or about 3% of each nations GDP. However,...

Download Free -or- to Buy Printed Copies

Hybrid Zinc Coatings: Specifying HDG + TSZ

Hot-dip galvanizing (HDG) and thermal spray zinc (TSZ) are two proven zinc coating corrosion protection systems, each offering unique advantages depending on project requirements. This guide provides a practical framework for specifying HDG, TSZ, or...

Hot-Dip Galvanized Reinforcing Steel: A Specifier's Guide

Repairing damage caused by corrosion costs billions of dollars annually. One significant contributor to the corrosion problem is decaying reinforcing steel bar (rebar), which causes staining, cracking, and spalling of concrete structures throughout...

Download Free -or- to Buy Printed Copies

Suggested Specifications for Hot-Dip Galvanizing

A suggested specification in CSI format for hot-dip galvanizing after fabrication. This guide aids in developing a better hot-dip galvanizing specification. MS Word Document - 13 pages. 2022. Not for sale. Available for Download Only.

Suggested Specification for Preparing Hot-Dip Galvanized Steel Surfaces for Painting

A suggested specification in CSI format for hot-dip galvanizing after fabrication. This guide aids in developing a better hot-dip galvanizing specification. MS Word Document - 9 pages. 2022. Not for sale. Available for Download Only.

Suggested Specifications for Hot-Dip Galvanized Reinforcing Steel

A suggested specification in CSI format for hot-dip galvanizing after fabrication. This guide aids in developing a better hot-dip galvanizing specification. MS Word Document - 13 pages. 2022 Not for sale. Available for Download Only.

Galvanizado en Caliente para Protección contra la Corrosión: Guía del Especificador

La corrosión y la reparación del daño por corrosión son problemas multimillonarios: las últimas estimaciones muestran que la corrosión metálica le cuesta a Estados Unidos aproximadamente $423 mil millones ($52 mil millones en Canadá), o cerca del 3%...

La Galvanisation à Chaud Pour la Protection Contre la Corrosion

La corrosion et la réparation des dommages dus à la corrosion représentent un problème de plusieurs milliards de dollars : les estimations les plus récentes font état d’un coût de la corrosion métallique aux États-Unis avoisinant les 423 milliards...

Acero de Refuerzo Galvanizado en Caliente: Guía del Especificador

La reparación del daño causado por la corrosión cuesta miles de millones de dólares al año. Un importante contribuyente al problema de la corrosión es la barra de acero de refuerzo (barra secundaria) en descomposición, que provoca el manchado, el...