Search Results:
This listing only shows the dimensions of the galvanizer's kettle (bath), and does not indicate the maximum material size that can be galvanized. Please contact the galvanizer for more information on capacity limits.
Galvanizers:
AZZ Galvanizing - Kennedale
1530 Gilman Rd
Kennedale,
TX
76140
United States
Phone: (817) 572-2280
Website
Kettle(s) (L × W × D):
55' x 7' x 7'6"
Zinkpower USA
PO Box 2140
WEATHERFORD,
TX
76088-7227
United States
K-T Galvanizing Co. - Venus
AZZ Galvanizing - Crowley
200 N Beverly
Crowley,
TX
76036
United States
Phone: (817) 297-4361
Website
Kettle(s) (L × W × D):
58' x 7'6" x 10'
AZZ Galvanizing - Plymouth
2631 Jim Neu Dr
Plymouth,
IN
46563
United States
Phone: (574) 935-4500
Website
Kettle(s) (L × W × D):
45' x 6' x 8'
Sabre Galvanizing
8669 E Hwy 67
Alvarado,
TX
76009
United States
Kettle(s) (L × W × D):
65' x 9' x 11'
South Atlantic LLC - Shannon Plant
61 County Road 520
Shannon,
MS
38868
United States
Phone: 662-601-4108
Website
Kettle(s) (L × W × D):
58' x 7'6" x 9'6"
AZZ Galvanizing - Nashville
3201 Elkins Ave
Nashville,
TN
37209
United States
Phone: (615) 297-9581
Website
Kettle(s) (L × W × D):
51' x 6'6" x 8'6"
AZZ Galvanizing - Louisville
6310 Kenjoy Dr
Louisville,
KY
40214
United States
Phone: (502) 367-6146
Website
Kettle(s) (L × W × D):
42' x 5' x 7'