![Wisconsin DOT Favors Duplex Coatings](/images/icon-block-kbase.jpg)
Wisconsin DOT Favors Duplex Coatings
In a recently released paper by the Wisconsin DOT, research findings suggest painting over galvanizing to be the superior corrosion and aesthetic coating system for bridges.