Cotton Bowl Renovation
Dallas, TX United States | 2008
2008
Menu • Quick Links • Search
The tropic marine environment of Boca Raton Florida was the primary factor of choosing hot-dip galvanizing (HDG) as the corrosion protection for this project. HDG's durable finish as well as limited touch up at the jobsite provided a seamless erection process in a time sensitive schedule. Fabricator and galvanizer worked closely to insure proper scheduling for delivery to the site. The HDG structure will guarantee many years of service before first maintenance.
2011
Newly Complete
Recreation & Entertainment
Tropical Marine
Boca Raton, FL United States
Coating Durability, Corrosion Performance, Life-Cycle Cost, Prior HDG Experience, Turnaround Time
100% of the super-structure for this stadium was HDG in addition to all of the light poles and assemblies.
Steel: 1800
HDG: 1800
Paul Ohlman, 502-634-3626, Plant Manager
Dant Clayton Corporation
Thank you! Your vote has been accepted.