Alligator Reef Lighthouse Replica
Monroe,Isla Morada, FL United States | 2013
Menu • Quick Links • Search
Hot-dip galvanizing was chosen for the supporting steel frame of the artistic pavilion structure along with the concrete reinforcing steel as needed to ensure the long term integrity of the overall concrete structure. With the internal supporting elements being hot-dip galvanized, there are no concerns for any future corrosion or maintenance problems.
2013
Newly Complete
Artistic
Recreation & Entertainment
Tropical Marine
Doral, FL United States
Coating Durability, Corrosion Performance, Life-Cycle Cost, Quality of HDG, Sustainability
Internal structure steel supporting frame (Raw Steel 20.24Tons/Galv. 22 tons) Concrete reinforcing steel-rebar (Raw steel 9.34Tons/ Galv 10.15 tons)
Steel: 29.58
HDG: 29.58