Archimedes of Syracuse
Omaha, NE United States | 2008
Menu • Quick Links • Search
The harsh southern weather in Suwanee, Georgia, could make a steel statue rust within months. Hot-dip galvanizing will allow the beautiful project to be rust free in the years to come. This project is very visible to the public, and galvanizing was the look they were after. It is located right in front of Suwanee City Hall.
2012
Newly Complete
Artistic
Suburban
Suwanee, GA United States
Aesthetics, Coating Durability
The entire project: The rock, wings, and the statue itself.
Steel: .6
HDG: .6
City Hall, Suwanee, GA
Jake Potter
V&S Amboy Galvanizing