Hot Dip Galvanizing was selected for Coating Durability because the project is in a high profile area and final restoration of the facility is in a high visibility area. The visual appearance was also very important, as this is the signature piece of the entire restoration of the Everett Memorial Stadium, which was over 80 years old.
2012
Newly Complete
Duplex Systems
Recreation & Entertainment
Suburban
Everett, MA United States
Aesthetics, Coating Durability
The gates were galvanized and then painted.