Distillery Gates
Woodford County, KY United States | 1996
1996
Menu • Quick Links • Search
Iron Masters needed great quality galvanizing for a highly visible project. Southern provided that quality and made the powder coating process that much easier on the customer.
HDG was vital to this project due to the durability and time to first maintenance. With Iron Masters being a local fab shop in Maryland they couldn't afford to keep flying out to Colorado every time there was a coating issue with the project. The decision was made to galvanize and powder coat it so that the life cycle would last well into the future. These fence panels act as the border fence for an upscale neighborhood, so they wanted the best iron work and coating available.
Newly Complete
Duplex Systems
Suburban
Denver, CO United States
Coating Durability, Corrosion Performance, Sustainability
50 Fence Panels, made of solid square bar welded together, ranged in size from 8' long to 10' long.
Steel: 15
HDG: 15
Iron Masters Inc
Southern Galvanizing Company