Worcester Psychiatric Hospital

In the harsh winters of Massachusetts, corrosion performance and coating durability are very important.

This Hospital is being brought up to modern use. There was a design issue the galvanizer had to overcome for the project to be successful.

The steel also had to be epoxy primered after hot-dip galvanizing in which the galvanizer had to be able to accomplish.

View Larger Image

Worcester Psychiatric Hospital

View Larger Image

Worcester Psychiatric Hospital

View Larger Image

Worcester Psychiatric Hospital

View Larger Image

Worcester Psychiatric Hospital

View Larger Image

Worcester Psychiatric Hospital

View Larger Image

Worcester Psychiatric Hospital - Aerial View

View Larger Image

Worcester Psychiatric Hospital - Aerial View

Project Specifics

Year Galvanized
2011
Sector(s)
Building & Architecture
Duplex Systems
Environment
Industrial/Urban
Location
Worcester, MA United States
Reason for Galvanizing
Coating Durability, Corrosion Performance,
Components Galvanized
Canopy over the entrance way to the hospital
Tonnage/Size
Steel: 55
HDG: 55

Project Members

Owner
Gilbane Construction
Fabricator
Cives Steel
Member Galvanizer(s)
V&S Taunton Galvanizing LLC