Careful handling by the galvanizer ensured a pristine coating. The galvanizer guaranteed this coating to the artist and homeowner and delivered - taking only a couple of hours, from start to finish, to move the gate through the galvanizing process.
The artist/blacksmith has learned that hot-dip galvanizing is the only coating that keeps his work from corroding. He said, Artwork should last generations. Hot-dip galvanizing is the only process I have found that can do that.