Oxbow Carbon & Materials Crusher
Long Beach, CA United States | 2012
Menu • Quick Links • Search
Upon completing the fabrication of the off shore drilling rig saw the owner asked "What can we do to minimize corrosion?" The only answer for this saw that is used under the salt water of the Gulf of Mexico was hot-dip galvanizing (HDG).
The fabricator and designers called on the galvanizer to provide information on corrosion protection, specifications and venting recommendations. Without any prior experience the customers were impressed with the initail support, quality and quick turnaround. They also commented on the impressive appearance of the galvanizing surface. The competitive price of galvanizing compared to paint, the expected maintenance-free life and resulting life-cycle costs made HDG the perfect choice.
2011
Newly Complete
Original Equipment Manufacturing
Tropical Marine
Red Wing, MN United States
Coating Durability, Corrosion Performance, Ease of Specifying
The entire framework of the 40" articulating saw was galvanized.
Steel: 5.6
HDG: 5.6
Mactech Offshore-Lafayette, LA
Mactech Onsite Machining Services-Red Wing MN
Neufeld Industrial Services- Red Wing MN
Innovation By Design-Owatonna, MN
AZZ Galvanizing - Winsted
Thank you! Your vote has been accepted.