A total commitment to providing the best corrosion protection available resulted in the galvanizing of this woodyard crane, the first of its kind. The complex design of the crane is usually not compatible with hot-dip galvanizing. However, designer, engineer, and galvanizer worked together to redesign the units for maximum corrosion protection. This innovative design launches the paper industry into a whole new level of corrosion protection.
Newly Complete
Original Equipment Manufacturing
Industrial/Urban
Moundville, AL United States
Corrosion Performance
All steel excluding the parts of the operators cab.