Located just a few short miles from the rugged west coast of British Columbia's Vancouver Island, the Distric of Ucluelet needed a durable coating to provide corrosion protection against the harsh climate of the Pacific Northwest's "Wet Coast". A duplex coating would ensure many years of maintenance-free protection and ensure the newly installed welcome sign will provide an attractive welcome greeting to visitors and residents alike.
2013
Newly Complete
Artistic
Duplex Systems
Temperate Marine
Ucluelet, BC Canada
Corrosion Performance, Life-Cycle Cost
3 Curved sign panels, individual letters, sign posts and all hardware.
Steel: 4
HDG: 4