Belmont Station
Chicago, IL United States | 2007
Menu • Quick Links • Search
The durability and maintenance free properties of hot-dip galvanized steel was chosen to withstand the extreme winters in Calgary.
2014
Newly Complete
Bridge & Highway
Transportation
Suburban
Calgary, AB Canada
Coating Durability, Corrosion Performance, Life-Cycle Cost
Guardrail, Pedestrian pipe bridge structures (4), Structural support cross members, Decorative light posts, bolts & hardware
Steel: 150
HDG: 150
Calgary Transit
City Of Calgary
John Huska
Cougar Metal
Silver City Galvanizing, Inc.