The city of Varennes, located on the Montreal's south shore, has invested 2 million dollars to renew their parks and recreation infrasturture for their 350th anniversary. The project included the construction of a bicycle and pedestrian trail along the St-Lawrence river. The bridge links the village bike path to the one along the St.Lawrence River.
Hot-Dip Galvanizing is the favorite choices or architect and engineers in Quebec when it comes to infrastrure as we are faced with harsh winter condition. The use of salt and chemicals to remove ice on it can accelerate the corrosion of any unprotected surface. This project was made to last and keep its integrety throughout many winter cycles.
Newly Complete
Recreation & Entertainment
Industrial/Urban
Varennes, QC Canada
Corrosion Performance, Life-Cycle Cost, Quality of HDG
Most of the structure was galvanized and the hands were run.
                                                                            Steel: 22
                                                                                                                HDG: 20
                                                                    
                                                    Simon Couture
                                                    Soudure M. Couture & fils inc                                                
                                                                                    AZZ Galvanizing - Galvan Metal
                                                                            