Electric utilities, municipalities, telecommunication companies & cable companies throughout North America have faced a common, yet unavoidable problem: The challenge of Installing wood poles in a rock foundation for transmission and distribution. This undertaking can prove extremely costly, particularly in remote, hard-to-reach areas.
It is essential that the product be able to withstand harsh weather year-round with minimal maintenance.
A revolutionary product engineered and tested by an engineer in Candiac, Quebec offers a cost effective solution to this problem.  The Rock Anchor is a very simple, robust economical system which allows the base of a wood pole to remain above grade once installed.  The Rock Anchor can be installed in 3, 4, or 5 leg configuration depending on the width of the wood pole.
The Rock Anchor is most often installed in remote, rocky ares that are difficult to access. It is essential that the product be able to withstand harsh weather year-round with minimal maintenance. Hot-dip galvanizing ensures the longevity of the product: each leg is hot-dipped galvanized to ensure durability and maintenance-free corrosion protection. Once installed, thanks to the hot-dipped galvanizing process, the Rock Anchor will last the entire life span of the pole.
2014
Newly Complete
Electrical, Utility & Communication
Original Equipment Manufacturing
Rural
Montreal, QC Canada
Coating Durability, Corrosion Performance, Prior HDG Experience
The complete item (Rock Anchor) is HDG