These towers, each weighing two tons, (1.8 tonnes), are temporary communication solutions most appropriate for microwave, PCS, cellular, SMR, contingency planning, disaster recovery, and other multi-media applications.
They provide customers with emergency needs on a very high profile basis. Each section was galvanized as one piece. This tower product is unique because not many companies provide them in a single unit. The towers are galvanized, with all the tower section assembled within one another. The towers must be galvanized in a way that the tower sections do not adhere to each other. The coating needed to have an aesthetic appearance because the towers are extremely visible to the public.