Hot-dip galvanizing extends the operational life and reduces maintenance of every Zamboni Ice Resurfacing machine. The Zamboni ice resurfacing machine is a true industry standard that utilizes hot-dip galvanizing to protect the machines main components and condenser tank. The galvanized areas serve as barrier protection for a constantly damp environment.
Newly Complete
Original Equipment Manufacturing
Temperate Marine
Paramount, CA United States
Corrosion Performance
Condenser tank.