Salt Water Filter Pod
Center, TX United States | 2011
Menu • Quick Links • Search
While most of us eat our hamburgers and steaks with nary a thought about the cow that provided it, Moly Manufacturing sees things differently. Farmers are responsible for far more than most of us realize when it comes to beef. We assume it is safe when we pick up a roll of ground beef from the supermarket. Giving a cow a necessary immunization never crosses our mind.
Special caution was taken to ensure no metal on metal contact occurred that would scare the animal...
Giving livestock a shot of anything is quite a feat. The animal is not going to be cooperative and when it moves in reaction to the injection, the animal and the person administering the shot could be injured. Moly MFG saw the need for a safe environment for both the animal and the injector. Moly Manufacturing thought of everything when creating the Silencer. They took into account every situation that could happen. There are parts that prevent the cow or other livestock from laying down in the chute.
There are safety measures that hold the livestocks head in place, so that no injury happens to the animal while a shot is being administered. Special caution was taken to ensure no metal on metal contact occurred that would scare the animal, thus the name, Silencer. The Silencers longevity is assured by hot dip galvanizing.
2015
Newly Complete
Food & Agriculture
Original Equipment Manufacturing
Rural
Lorraine, KS United States
Coating Durability, Corrosion Performance, Ease of Specifying, Life-Cycle Cost, Quality of HDG, Sustainability
Miscellaneous parts of the cattle chute that make up its basic framework.
Steel: 2
HDG: 2
Ray Stern
Moly Manufacturing
Mike Kotik
Valmont Coatings Salina Galvanizing
Micah Copeland
Valmont Coatings Salina Galvanizing
Rod Morgan
Valmont Coatings Salina Galvanizing
Valmont Coatings - Salina Galvanizing
Thank you! Your vote has been accepted.