Nevada Solar One Solargenix Energy
Boulder City, NV United States | 2006
2006
Menu • Quick Links • Search
The solar arrays will be exposed to harsh weather conditions throughout the year. Hot-dip galvanizing was chosen for this project due to its longevity and durability. There are many exposed steel components on the solar array supports and HDG provides protection for the edges and corners as well as the inside of the tubular sections. The dishes are guaranteed to last at least 25 years and by utilizing galvanizing for corrosion protection, the dish supports will be maintenance free for decades exceeding the projects life expectancy.
2013
Newly Complete
Electrical, Utility & Communication
Rural
Tooele, UT United States
Coating Durability, Corrosion Performance, Ease of Specifying, Life-Cycle Cost, Prior HDG Experience, Sustainability
Dish Center Weldments, Post Weldments, Boom Arms, Dish Arm Extensions, & Counter Weight Pins
Steel: 98
HDG: 98
United States Army
Infinia Corporation
Richards Sheet Metal Works, Inc.
CDM Constructors, Inc.
Hunt Electric
Valmont Coatings - Intermountain Galvanizing