Gheens Planetarium
Louisville, KY United States | 2001
Menu • Quick Links • Search
Rooftop furniture will be exposed to the elements year-round, and in Nebraska, this means extremes of all weather types. The durability of hot-dip galvanizing is an excellent choice to ensure a maximum life-cycle for the customer. Given that Lincoln is a university town, the "green" aspects of hot-dip galvanizing further enhance the benefits of the project and are a good match for the community.
2012
Newly Complete
Artistic
Building & Architecture
Recreation & Entertainment
Industrial/Urban
Lincoln, NE United States
Coating Durability, Corrosion Performance
(3) Benches
(6) Chairs
(4) Coffee tables
(1) Double chaise lounge chair
(20) Chaise lounge chairs
                                                                            Steel: 4.5
                                                                                                                HDG: 4.5
                                                                    
                                                    Emily Brodersen
                                                    TMCO, Inc                                                
                                                                                    Valmont Coatings - Valley Galvanizing
                                                                            