All fencing surrounding the stadium is hot-dip galvanized. While the galvanizer was processing the initial fence shipment, trucks were waiting to deliver more to the galvanizer. Overall, 600 tons (544 tonnes) of steel were hot-dip galvanized in a matter of days. The fence is 12 ft (3.7 m) tall and surrounds the entire stadium. After galvanizing, the fence was painted, adding an aesthetically pleasing appearance and durability to the fencing. In all, including handrail, there is over one mile (1609 m) of hot-dip galvanized fencing.
Newly Complete
Duplex Systems
Recreation & Entertainment
Industrial/Urban
Louisville, KY United States
Corrosion Performance
The fence surrounding the outside of the stadium.