This job was 9 million pounds that needed to be completed in less than 8 weeks in order for the customer to secure the project. Hot dip galvanizing was the only coating system that could make this happen.
With the weather and winters of Minnesota, plus the storied history of galvanizing in the Solar industry there was only one choice for the protection of the steel.
2015
Newly Complete
Electrical, Utility & Communication
Suburban
North Branch, MN United States
Coating Durability, Corrosion Performance, Sustainability
All Structural Post, frames, Louvers, and rails.
Steel: 4500
HDG: 4500
Steel of West Virginia
Marshall Steel
V&S Detroit Galvanizing LLC
V&S Memphis Galvanizing LLC