Corrosion in a salt storage facility is at a maximum. Hot dip galvanizing was the best choice for protection against corrosion. There was no paint system that could perform as well in this environment. HDG was easy to specify and the life cycle cost sealed the deal. The quality of coating confirmed that hdg was the right choice.
2011
Newly Complete
Building & Architecture
Industrial
Industrial/Urban
Saugerties, IN United States
Coating Durability, Corrosion Performance, Ease of Specifying, Life-Cycle Cost, Quality of HDG
The structural support beams and cross members were galvanized.
                                                                            Steel: 76