Black Sea Export Terminal
Constanta, United States | 1999
1999
Menu • Quick Links • Search
The Kodiak Ferry dock is located on the waterfront of Kodiak, Alaska in Kodiak-Chenega Bay. The 126 tons of steel to create this dock was galvanized to ensure maximum long term corrosion resistance on steel which is submerged in salt water 100% of the time.
As a multi use dock, it is a place to load and unload ferry riders, fishing gear and transfer bulk fuel.
2015
Newly Complete
Bridge & Highway
Industrial
Water & Marine
Temperate Marine
Kodiak, AK United States
Coating Durability, Corrosion Performance, Sustainability
All steel product for assembly of the terminal were galvanized.
Steel: 126.5
HDG: 126.5
Robert Webster
Rainier Welding
Andrew Romine
Pacific Pile & Marine
Seattle Galvanizing Company