Lesco Design & Manufacturing, a trusted leader in the manufacturing industry for over 60 years, has built its reputation on engineering solutions that withstand the test of time and use. With a primary focus on serving the automotive industry, Lesco is known for delivering quality components that meet the sector's stringent demands. The company sought a reliable, long-lasting solution for its heavy-duty loading ramps, which are critical to material handling systems within the automotive supply chain. These ramps required enhanced durability, corrosion resistance, and the capacity to endure extreme conditions encountered during vehicle transport and logistics operations.
By addressing the unique challenges of automotive logistics and material handling systems, the galvanized ramps provide a durable and reliable solution capable of withstanding some of the most demanding conditions.
To ensure these specialized ramps met and exceeded the rigorous demands of their applications, they were hot-dip galvanized, a process that provides exceptional durability and corrosion resistance. Each ramp was constructed with galvanized steel for unmatched protection, heavy-duty drive axles capable of withstanding repeated use in high-stress environments, and I-beam frame construction engineered for strength and reliability under immense loads. These features made the ramps versatile enough to handle the precision required for loading passenger vehicles, as well as heavy-duty applications such as equipment transport within the automotive industry.
The galvanizing process was chosen for its unparalleled ability to protect steel in harsh environments. The ramps were coated, ensuring superior corrosion resistance critical for outdoor or high-moisture environments where exposure to salt air, chemicals, and extreme weather conditions accelerates metal degradation. This process provided an extended lifespan, reducing the need for maintenance and replacement over time, and enhanced performance to maintain structural integrity under heavy use in challenging conditions often faced during automotive transport and handling operations.
Through this galvanizing solution, Lesco delivered loading ramps that meet the highest industry standards for durability and reliability. The finished ramps not only provided superior performance but also reinforced the company’s ability to support the automotive sector with reliable, high-quality material handling systems essential for vehicle transport.
This project highlights the transformative role of galvanizing in enhancing the performance and longevity of critical components. By addressing the unique challenges of automotive logistics and material handling systems, the galvanized ramps provided a durable and reliable solution capable of withstanding some of the most demanding conditions, reinforcing Lesco’s reputation for quality and innovation.
Newly Complete
Original Equipment Manufacturing
Industrial/Urban
LaGrange, KY United States
Corrosion Performance, Ease of Specifying, Prior HDG Experience, Sustainability
Ramp