Romeoville Aggregate Screening Plant
Romeoville, IL United States | 2010
Menu • Quick Links • Search
Having used both paint and hot-dip galvanizing on previous projects, both the manufacturer and the owner knew that only hot-dip galvanizing can withstand the harsh environment of a stone processing plant.
2013
Newly Complete
Industrial
Industrial/Urban
Lexington, KY United States
Coating Durability, Corrosion Performance, Ease of Specifying, Prior HDG Experience, Quality of HDG
Hoppers, conveyors, stairs, chutes, and all structural steel.
Steel: 235
HDG: 225
Process Machinery Inc
Process Machinery Inc
Process Machinery Inc
AZZ Galvanizing - Louisville
AZZ Galvanizing - Nashville