Darkened Light Fixture
Dallas, TX United States | 1998
Menu • Quick Links • Search
As a part of the revitalization efforts taking place in downtown Omaha, the Greater Omaha Chamber of Commerce sought materials which would be durable, recyclable and aesthetically pleasing in an urban environment. Hot-dip galvanizing allowed them to meet all of these requirements. Coupled with the designs produced by Emerging Terrain, the durability of hot-dip galvanizing ensures a cost-effective, environmentally friendly, and attractive addition to the area.
2012
Newly Complete
Artistic
Building & Architecture
Duplex Systems
Industrial/Urban
Omaha, NE United States
Aesthetics, Coating Durability, Ease of Specifying, Life-Cycle Cost, Sustainability
Steel frame platform, Corrugated metal Trug body
Steel: 3
HDG: 3
Cydney Franklin
Greater Omaha Chamber of Commerce
Valmont Coatings - Valley Galvanizing
Thank you! Your vote has been accepted.