Broadway Bridge
Boston, MA United States | 2002
Menu • Quick Links • Search
More than 120 tons of steel, including tubular railing, supports and mounting plates, were hot-dip galvanized for corrosion protection. The galvanized coating will keep the railing aesthetically appealing for decades in the corrosive roadside environment.
Newly Complete
Bridge & Highway
Temperate Marine
Indianapolis, IN United States
Corrosion Performance
Tubular railing, supports and mounting plates.
Steel: 120
HDG: 120