The pergola and bus shelter, railings, and miscellaneous steel were painted-over hot-dip galvanized steel, giving the Federal Reserve Bank in Minnesota a demure decor, while complimenting the surrounding buildings and stonework.
...it was economical to use a duplex system.
The Federal Reserve Bank is saving money; it was determined that over the life of the outside structures it was economical to use a duplex system. This system blends nicely with the outside environment and will continue to do so for decades to come.