The customer chose to have the steel for this project hot-dip galvanized for aesthetics and sustainability reasons. The gazebo at the Columbia Canal will be a highly visible attraction located along the newly constructed boardwalk providing additional character to this historic site. The customer was focused on ensuring the gazebo added effortless beauty to this historic site while minimizing maintenance costs.
2012
Newly Complete
Building & Architecture
Water & Marine
Industrial/Urban
Columbia, SC United States
Aesthetics, Coating Durability, Corrosion Performance, Ease of Specifying, Life-Cycle Cost, Sustainability
Steel beams, angles, and tubes.
                                                                            Steel: 2.36
                                                                                                                HDG: 2.5
                                                                    
                                                    Scott Campbell
                                                    The Metal Works, Inc.                                                
Studio 2LR
Cherokee, Inc
                                                                                    Valmont Coatings - Columbia Galvanizing
                                                                            