Although more cities and municipalities are requiring unobtrusive cell tower designs and appearances, hot-dip galvanizing continues to be the choice for corrosion protection. This is especially true for galvanized cell towers covered with a rubber bark and located in coastal and highly corrosive environments. Just as for a duplex system, the zinc provides and "under-bark" protection on the entire pole surface, around the many limb brackets welded in place, and complete coverage inside the cell tower pole itself. Special handling of each 12,000 pound pole was required to deliver a quality framework for these "not-so-real" palm and deciduous trees.
Newly Complete
Electrical, Utility & Communication
Original Equipment Manufacturing
Rural
, CA United States
Coating Durability
The pole and cell tower signaling parts.
Steel: 6
HDG: 6
W.S.C. Engineering
Zinkpower USA - Portland