Menu • Quick Links • Search
The goal of the Capital Crossroads Special Improvement District was to beautify the area surrounding Ohios State Capitol Square. In conjunction with the City of Columbus and a local artist, this has been done with the addition of these 72 planters.
The planters required an aesthetically pleasing coating, but needed to withstand the harsh environment of installation just a few feet from the street. The powder coating over hot-dip galvanizing system provided the ultimate solution for both of these necessities.
2013
Newly Complete
Duplex Systems
Industrial/Urban
Columbus, OH United States
Aesthetics, Coating Durability
All of the planters.
Steel: 25
HDG: 25
City of Columbus
City of Columbus
John Sunami
Stewart Iron Works
V&S Columbus Galvanizing