South Campus Central Chiller Plant at The Ohio State University
Columbus, OH United States | 2012
2013
Menu • Quick Links • Search
The structure is in the city-centre of Turin, Italy. Seven buildings at the University of Turin were completed with galvanized steel structures of 1,000 tons.
The Campus Luigi Einaudi is in 45,000 sqm inside the green in Turin that contains more than 620,000 Books for 8,000 students from all around the world.
The luminous structure utilizes hot-dip galvanized steel with a suspended roof that saves 20 % of the electrical power required for the building.
2013
Newly Complete
Building & Architecture
Suburban
Turin, Italy
Life-Cycle Cost, Sustainability
The Luminous structures.
Steel: 3500
HDG: 1000
arch. Benedetto Camerana
Foster & Partners
Prof. Sergio Roda
University Library of Turin
Arch. Pichler
Stahlbau Pichler
Galvanizer- Bordignon Group, Zincheria Valbrenta SPA
Thank you! Your vote has been accepted.