Cape Disappointment Wave Barrier
Ilwaco, WA United States | 2006
                                                    
                                                                                                            2006
                                                                                                    
Menu • Quick Links • Search
The Tuffboom is a floating barrier used worldwide to cordon off waterways. They are commonly used to protect dams from debris and to keep boaters safe and out of spillways and hydro-electric water intakes. However, in addition to protecting the casual boater, they are also used to keep terrorists away from potential targets. Since the attack on the USS Cole, thousands of feet of these barriers have been installed at US naval bases worldwide.
The systems require a tough coating as they are in corrosive marine environments...
The systems require a tough coating as they are in corrosive marine environments and are designed to stop a 15,000 pound speedboat going 50 knots. Hot-dip galvanized steels superior corrosion protection in marine environments will help keep US Naval personnel, and leisure boaters safe well into the future.
Newly Complete
Water & Marine
Tropical Marine
Throughout North America, United States
Corrosion Performance
Channel frames, screens, connectors, and cable.
                                                                            Steel: 35
                                                                                                                HDG: 35
                                                                    
Worthington Products