LMT Septic Tank
Galva,, IL United States | 2006
Menu • Quick Links • Search
Since Tank Truck buyers fight tight budgets and require a product with an extended life span, Truck Works integrates hot-dip galvanized steel to provide its users a great advantage to the bottom line.
Thanks to the combined strength of paint over hot-dip galvanized steel, known as duplex coating, the tanks achieve a time to first maintenance 1.5 times longer than the sum of the individual coatings. These durable tanks are protected from corrosion by a rust-resistant hot-dip galvanized coating which protects the equipment from the inevitable scratches, dings, and dents associated with the harsh trucking environment. HDG will keep them trucking along corrosion free for decades.
Newly Complete
Original Equipment Manufacturing
Industrial/Urban
Phoenix, AZ United States
Coating Durability
Tank is 100% galvanized, ladders, plumbing and gates.