Wisdom Rides
Merino, CO United States | 2015
Menu • Quick Links • Search
Hot-dip galvanizing was chosen because of being exposed year round to the "Temperate Marine" environment of being located approximately 3/4 mile from the Atlantic Ocean. Hot-dip galvanized steel's corrosion resistance is proven in these various environmental conditions.
Hot-dip galvanized steel's corrosion resistance is proven in these various environmental conditions.
Durable and maintenance free for many years to come, along with corrosion protection, is vital to the overall performance and safety of the structure. Aesthetics of galvanized steel remains constant, without the need for costly reapplication of paint.
The life-cycle cost of galvanizing versus paint made galvanizing the most practical and economic choice and allowed for faster assembly of loose pieces not requiring any touch up as with painted steel.
2015
Newly Complete
Recreation & Entertainment
Temperate Marine
Myrtle Beach, SC United States
Coating Durability, Corrosion Performance, Life-Cycle Cost, Quality of HDG, Sustainability
W Beams, Channels, Round Tubes, Angles, Plates, Handrails, Solid Picket Fencing<br />
Steel: 203
HDG: 203
Bender and Associates
Bender and Associates
Elvis Welding Service, Inc.
Chris Bethea, Rittner Will and Chad Will
Rittner Will
Project Manager
Chad Will
Superintendent
Thank you! Your vote has been accepted.