Stevenage Railway Station Parking Garage Facade
Stevenage, United Kingdom |
Menu • Quick Links • Search
The Star is a 91-acre premier sports and entertainment district in Frisco, Texas that is also home to the world-famous Dallas Cowboys. Situated on 91 acres of land, The Star is a $2-billion, mixed-use development in Frisco, Texas.
The Star features over 1.5 million sq. ft. of office space; 225,000 sq. ft. of retail space including 23 restaurants and bars; a 12,000-seat, multi-use event center which expands to 22,000 seats for music events; a 300-key Omni Hotel with 15,000 sq. ft. of event space; a 170-key luxury apartment living center; and a 300,000 sq. ft. MOB component providing world-class sports medicine and research facilities.
Galvanizing is an ideal choice for a parking garage, where maintenance access can be challenging, and the structure needs to remain functional and safe with little disruption.
Hot-dip galvanizing was specified for this project due to its exceptional ability to provide long-term corrosion protection and little to no maintenance required. Galvanizing is an ideal choice for a parking garage, where maintenance access can be challenging, and the structure needs to remain functional and safe with little disruption.
Furthermore, hot-dip galvanizing offers versatility and provides a uniform, durable coating that adheres well to complex geometries, ensuring that all parts of the garage are effectively protected from corrosion. This consistency in coating quality ensures long-term reliability and strength. Hot-dip galvanizing is an environmentally friendly option. This aligns with sustainability goals, especially for large infrastructure projects like parking garages, where durability and environmental responsibility are key considerations.
Newly Complete
Transportation
Industrial/Urban
Frisco, TX United States
Aesthetics, Coating Durability, Corrosion Performance, Ease of Specifying, Life-Cycle Cost, Prior HDG Experience, Quality of HDG, Sustainability
Panels and frames for parking garage
HDG: 117
American Steel & Aluminum Co Inc
HKS
Zinkpower USA - Waco