Mobile Training Tower for First Responders
Hawkinsville, GA United States | 2010
2010
Menu • Quick Links • Search
Rosenbauer has discovered that hot-dip galvanized (HDG) steel is the most cost efficient coating solution for maintenance free ladders in their industry. HDG was specified for the complete coverage of the immersion process and for the outstanding corrosion protection.
Rosenbauer guarantees the corrosion resistance on the inside and outside of their aerials...
The entire interior and exterior areas are protected with HDG. The intermetallic bond of the zinc as a result of HDG is approximately ten times greater than the adhesion of paint to the underlying steel. Rosenbauer guarantees the corrosion resistance on the inside and outside of their aerials for 25 years. Rosenbauer aerial ladders will outlast any aerial in the industry.
2011
Newly Complete
Original Equipment Manufacturing
Industrial/Urban
Fremont, NE United States
Aesthetics, Coating Durability, Corrosion Performance, Life-Cycle Cost, Prior HDG Experience, Quality of HDG, Sustainability
Aerial ladder sections, stabilizers and torque tube boxes.
Steel: 135
HDG: 135
Rosenbauer Aerial
Valmont Coatings - Valley Galvanizing
Thank you! Your vote has been accepted.