Premier Scaffold Solutions reinvented the mobile scaffold industry in 2009 with their ProSeries Mast Climber. The ProSeries Mast climber makes it easier to replace aging mast climbers, because of its modular bridging being compatible with other mast climbers on the market. When mast climber owners need to upgrade their power units, the ProSeries will be their best option based on quality, price and the longevity of a galvanized product.
When mast climber owners need to upgrade their power units, we feel the ProSeries will be their best option based on quality, price and the longevity of a galvanized product.
Most in the construction industry know that the equipment used on the job site goes through mush trial and tribulation on any given day. Being transported from site to site, stored for long periods of time in summer's heat and winter's cold, and worked to the brink in order to meet the project deadlines. Mobile scaffolding is no different, as it allows the masonry crews, glass installers and exterior carpenters to move up and down the outside of any facade.
Durability and protection from the elements is a must as the mobile scaffolding is relied upon to lift workers high into the air. Hot-dip galvanizing protects the scaffolding in all conditions and climates. The ability to coat the inside and the outside of the tubular deck components help to ensure the lifts will continue to safely carry their crews. The 3,600 psi metallurgical bond of galvanizing will protect the steel from the abuses of any construction job site. From it's very first lift into the sky to its 10,000th, the ProSeries Mast Climber will be as strong as the day it was built thanks to hot-dip galvanizing.
Newly Complete
Original Equipment Manufacturing
Industrial/Urban
Somerset, OH United States
Coating Durability, Corrosion Performance, Life-Cycle Cost, Turnaround Time
Pro Series mast climber scaffolding components made up of tube steel, diamond tread plate, angles, channels
Steel: 1
HDG: 1
Premier Scaffold Solutions