Casino Arizona at Talking Stick
Scottsdale, AZ United States | 2011
Menu • Quick Links • Search
Chosen to protect the structural steel from the damaging effects of the urban Chicago environment, hot-dip galvanized steel will keep the renovations at Presidents Plaza corrosion-free for 50+ years.
All 45 tons of structural steel and support bracings for the outdoor canopy at the plaza were galvanized, meaning the structure will require little or no maintenance for decades.
Newly Complete
Building & Architecture
Select Environment
Chicago, IL United States
Life-Cycle Cost
All structural steel and supports bracing the outdoor canopy.
                                                                            Steel: 45
                                                                                                                HDG: 45
                                                                    
                                                    Ken Worildy
                                                    Wright Heerema Architects                                                
Klein and Hoffman, Inc.
                                                                                    Valmont Coatings - Empire Galvanizing
                                                                            
Thank you! Your vote has been accepted.