Landa Mobile Systems LLC manufactures mobile utility towers and has customers internationally. Landa's Mobile Towers are deployed in emergency situations as needed all over the world. Larry Phillips, Operations Manager, decribes the reasons they choose Hot Dip Galvanizing over all other coating systems for their Mobile Towers.
"Our main reason for galvanizing is to create an all weather, all climate portable tower for our customers. We have a large number of clients that are in tropical climates with a lot of salt water in the air. Galvanizing is the solution to the surface protection issue. Our towers must be very dependable as they are used for emergency restoration of communication sites. It the tower is not 100% protected from the environment, it has a chance of failure with deployment is necessary. Over the years the galvanizer has been a trusted partner in taking care of all our Galvanizing as it has evolved with our customers needs."
2015
Newly Complete
Electrical, Utility & Communication
Industrial/Urban
Tulsa, OK United States
Coating Durability, Corrosion Performance, Sustainability
Expandable tower sections, and base supports.
Steel: 85
HDG: 85
Larry Phillips
Landa Moblie Systems
AZZ Galvanizing - Tulsa