Calipso Water Park
Limonges, ON Canada | 2009
                                                     2009
                                                                                                            2009
                                                                                                    
Menu • Quick Links • Search
The galvanizer hot-dip galvanized 168 tons (152 tonnes) of steel that was used for columns, beams, handrails and stairs for the 76-foot (23-meter) tall water slide, Juhranimo Falls, as part of the Six Flags Hurricane Harbor. A galvanized coating is ideal to protect the steel from mother nature's natural corrosive forces, particularly in a water park. In the past, steel waterslides have been painted or used wood supports. Seeing the quality and durability of Juhranimo Falls should encourage others to design their rides using hot-dip galvanized supports.
Newly Complete
Recreation & Entertainment
Temperate Marine
Jackson, NJ United States
Prior HDG Experience
Stairs, handrails, platforms, columns, all tower steel and support arms for fiberglass slides.
                                                                            Steel: 168
                                                                                                                HDG: 168
                                                                    
Pro Slide Technology
McKamish Chesapeake