Some of the most important infrastructure in a community is infrastructure most people never see. Beneath streets, sidewalks, campuses, and commercial developments, extensive networks of fiber-optic cable and telecommunications conduit carry the information communities depend on every day. These underground systems support businesses, schools, emergency services, and countless daily communications, yet they must remain accessible to technicians for installation, inspection, maintenance, and future expansion. Providing that access are utility vaults, pull boxes, and handhole assemblies manufactured for telecommunications networks such as AT&T. Jensen MetalTech fabricates the steel access systems incorporated into these precast concrete structures, with hot-dip galvanizing providing the corrosion protection necessary to help them withstand decades of exposure. The assemblies include heavy-duty welded steel frames integrated with traffic-rated precast concrete vaults, along with galva
There is no skyline-defining structure or dramatic architectural centerpiece associated with this project. Its importance is measured differently. These galvanized access systems become part of the everyday landscape, embedded in the streets and sidewalks people travel without a second thought. Their job is simply to remain safe, secure, and functional while protecting dependable access to the sophisticated communications networks operating beneath them.
The location of these access systems creates an especially challenging environment for fabricated steel. Installed at the intersection of above-ground and underground conditions, telecommunications access structures are continually exposed to moisture, road salts, irrigation runoff, UV exposure, and pedestrian and vehicular traffic. Hatch doors must also withstand repeated handling as technicians open and close the vaults throughout their service lives. Hot-dip galvanizing addresses these challenges by providing a tough, metallurgically bonded zinc coating over the fabricated steel. The coating protects exposed surfaces as well as edges, corners, welds, and other areas vulnerable to corrosion, while its abrasion resistance is well suited for components subjected to traffic, handling, and repeated use. Collectively, these characteristics provide a durable, low-maintenance corrosion protection system well matched to infrastructure that may remain in service for decades. By extending the service life of these
Newly Complete
Electrical, Utility & Communication
Industrial/Urban
Reno, NV United States
Coating Durability, Corrosion Performance, Life-Cycle Cost, Sustainability
The assemblies include heavy-duty welded steel frames integrated with traffic-rated precast concrete vaults, along with galvanized Traxplate and diamond-plate hatch doors that create a durable, slip-resistant access point at the surface.