We can say with certainty that today's world is full of uncertainties and ambiguity. The urge for short term results has obscured long term visions in many areas of business and life in general and we all have become way too used to instant gratification. However, there are areas of life and the economy, which must be protected from those trends, maintain and even double down on long term stability, extended performance, resilience and redundancy. One such area is America's critical energy infrastructure and back-up power generation.
How can a hospital function if a power outage suddenly hits during a storm? How will our data, stored on giant servers, be protected if the power fails? How do we protect the enormous amount of food stored in freezers and coolers throughout the nation when the utility infrastructure is compromised?
Answer - Distributed Power Generation and diesel or natural gas Gensets!
Durability & cost are the biggest factors in our customer decision to go with HDG.
When purchasing a Genset to provide backup power for hospitals, government institutions, data storage centers, food and beverage manufacturing and warehouses, office buildings, pipeline compressor stations, to name a few, the engineers and owners have to choose the coating system which will best protect their investment. One critical component of this investment is the core remote radiators used to cool the engine generator sets. Since those remote radiators are always exposed to the environment, whether marine, urban, industrial, tropical or rural, ensuring long maintenance free service is imperative. For this reason Young Touchstone - US manufacturer of Horizontal Core Remote Radiators decided to Hot Dip Galvanize and afford their customers the luxury of longevity, reduced total cost of ownership and quick turnaround! Indeed, the balance between durability and cost is what makes HDG the top choice metal coating system.
The vessels, tanks and all structural components of the Horizontal Core Remote Radiators are intricate and definitely challenging to galvanize. Working closely with Young Touchstone engineers the galvanizer was able to accommodate the complicated designs by relying on many years of experience and a touch of ingenuity. Achieving extended corrosion control over the design life of the components grants Young Touchstone a competitive edge, reaffirms their commitment to quality and leaves a lasting impact on the HDG market.
Newly Complete
Electrical, Utility & Communication
Tropical Marine
Nashville, TN United States
Corrosion Performance, Life-Cycle Cost, Sustainability
Horizontal Core Remote Radiator bodies and vessels.
                                                                            Steel: 20
                                                                                                                HDG: 20
                                                                    
Young Touchstone
                                                                                    AZZ Galvanizing - Chattanooga
                                                                            