This trailer manufacturer has taken a patent out on this particular type of trailer. The intent is to market it to utility companies all over North America. He needed a coating system that was durable as he has taken this to many areas and trade shows. The corrosion protection qualities is what he is promoting with this trailer.
2016
Newly Complete
Original Equipment Manufacturing
Industrial/Urban
Manheim, PA United States
Coating Durability, Corrosion Performance, Prior HDG Experience
The entire trailer, framing, wheel wells, and hitch.