Galvanized Steel was selected for the corrosion protection. They were concerned with corrosion staining over the years to come onto the stone, brick, and mason work that was to be done for all of the walkways. They liked the sustainability and were convinced a galvanized structure could be delivered painted to match the color scheme of the other steel in the area.
2015
Newly Complete
Bridge & Highway
Building & Architecture
Suburban
Fredrick, MD United States
Aesthetics, Corrosion Performance, Initial Cost, Prior HDG Experience, Sustainability
The entire Bridge, Rails, Garden Furniture, Lighting, and embeds.
Steel: 140
HDG: 140
Shannon Blanchard
Antietam Metals
HNTB-Urban Design and Planning
V&S Lebanon Galvanizing