Subdued Radiance (Lion Sculpture)
Keizer, OR United States | 2008
Menu • Quick Links • Search
The city of Oshawa set out to create an incredible full size moose chia pet. The gardener planned to wrap the frame in chicken wire and fill it full of seed bearing soil. The fabricator decided to galvanize the moose because it was supposed to be in a continuously damp environment.
After the moose was galvanized, the Head of Parks Commission came to see it. They decided to no longer use it as a chia pet because they fell in love with the look of the sculpture with the hot-dip galvanized coating. The town of Oshawa ended up being so proud of the sculpture, and they moved it to Town Hall.
The city was very happy with the moose but it would not have been the sculpture it is, without the help of a galvanizer with a kettle wide enough to fit the antlers. Oshawa shows a proud representation of Canadian wildlife with their new sculpture.
2016
Newly Complete
Artistic
Industrial/Urban
Oshawa, ON Canada
Aesthetics, Coating Durability, Corrosion Performance, Prior HDG Experience, Quality of HDG, Turnaround Time
The Entire Moose Sculpture (8 Tall x 10 Long)
Steel: .635
HDG: .635
ROBERT BRIERE
B.M WELDING (Custom Welding, Machining, CNC Profile Cutting & Forming)
Valmont Coatings
Thank you! Your vote has been accepted.