Pier 1 & Pier 21 Replacement
Norfolk, VA United States | 2002
2002
Menu • Quick Links • Search
The height above water is about five metres so it was essential to have a robust galvanized coating on all the exposed steel in order to withstand the marine environment. Aesthetics and long-term acceptance by the public also played a role in the selection of galvanized steel for this project.
2013
Newly Complete
Recreation & Entertainment
Water & Marine
Temperate Marine
Burlington, ON Canada
Aesthetics, Coating Durability, Corrosion Performance, Ease of Specifying, Prior HDG Experience, Quality of HDG, Sustainability
60 tons of 48" diameter x 40' long pilings and 138 tons of curved support beams, channel supports and handrails for the approach to the pier.
Steel: 200
HDG: 198
Deborah Franke
A.J. Braun Mfg. Ltd., Kitchener
Bermingham Construction, Hamilton
General Contractor
Graham Infrastructure, Calgary
Erector
All-Trade, Toronto
Consulting Engineer
Morrison, Hershfield