Arborea Magna stands as a magnificent work of metallic art that seamlessly integrates into its urban environment, brilliantly merging innovation with sustainability.
The volumetric design respects the maximum allowed heights ensuring that this piece of art integrates harmoniously to the urban surroundings without invading contiguous spaces. Arborea Magna combines innovation and sustainability which perfectly meets the artistic and functional visions consolidating itself as an icon in the park's landscape and emblematic for Buenos Aires city.
This 34-meter-high monument symbolizes the dialogue between nature, technology, and the environment. Made of 28 tons of HDG steel, 754 LED lights, and over 27,000 ceramic pieces, every design decision ensured seamless integration into the Innovation Park. Positioned along the boulevard’s longitudinal axis, it is easily visible to passersby. A 5% sloped ramp, meeting accessibility standards, allows visitors of all abilities to explore the structure, culminating in a viewpoint that offers an immersive experience of its textures and lights.
Key elements of the project include:
Arborea Magna is more than just a monument—it is a testament to the potential of modern materials and technology to create art that is both timeless and forward-thinking. It blends functionality with beauty, demonstrating how innovation and sustainability can come together to enrich urban landscapes and inspire future generations.
Newly Complete
Excellence Award Winners
International
Industrial/Urban
BUENOS AIRES, Argentina
Aesthetics, Coating Durability, Corrosion Performance, Life-Cycle Cost, Sustainability
Steel tubes, anchor plates, bolts, hardware (bolts and nuts) and steel plate.
Steel: 26
HDG: 28
GRUPO NH
Artist - NICOLA COSTANTINO
DRUETTA HNOS. S.A.